Brand Name : PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number : Waspaloy, UNS N07001, 2.4654, DIN NiCr20Co13Mo4Ti3Al, grade 685, ATG W1
Certification : SGS, TUV, BV, ISO, MTC
Place of Origin : China
MOQ : 800kg
Price : Negotiations
Payment Terms : T/T
Supply Ability : 50000KGS/Month
Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
Packaging Details : Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name : NiCr20Co13Mo4Ti3Al W-Nr 2.4654 Superalloy
Characteristic : Corrosion and Heat-Resistant
Heat treatment condition : +A, +W, etc
Processing methods : Peeled, Milled, etc
Available Shapes : Tubing, Steel plate, etc
Surface : Grinded, Black, etc
NiCr20Co13Mo4Ti3Al W-Nr 2.4654 Superalloy Waspaloy UNS N07001 Steel Bar
  
 Product Information
Waspaloy (UNS N07001) is a nickel-based superalloy that is capable of age-hardening and exhibits excellent strength at temperatures as high as 980°C. It is widely used as a forging material for the manufacture of gas turbine and aerospace components. Its strength is generally comparable to R41 alloy, and it outperforms the 718 alloy at temperatures above 650-705°C. Waspaloy is commonly used for high-temperature applications, particularly in gas turbines.
 Size Range
  
 Round bar / Wire rod (Diameter):8.0 mm to 500 mm
 Square bar / Flat bar: 5.0 mm to 500 mm
 Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
 Heavy/middle plate via hot rolled: T5 - 1000 mm X W8 - 1000 mm X L800-12000 mm
 Sheet steel via cold rolled: T5.0 - 8 mm X W5 - 1000 mm X L100 - 1000 mm
 Steel strip via cold rolled: T0.5 - 8 mm X W10 - 1000 mm X L (or in coil form)
 Length: Fixed length or random length or based on the customer's special requirement.
  
  
 Chemical Composition and standard
|   | NiCr20Co13Mo4Ti3Al / 2.4654 | ATG W1 | 
| -- | EN 10302-2008 | -- | 
| 
 C(%): 0.02~0.10 Cu(%): ≤0.5 Ti(%): 2.75~3.25 Co(%): 12.0~15.0 Al(%): 1.2~1.6 Fe(%): ≤2.0 Zr(%): 0.02~0.12 B(%): 0.003~0.01 
 | 
 C(%): 0.02~0.10 Cu(%): ≤0.1 Ti(%): 2.80~3.30 Co(%): 12.0~15.0 Al(%): 1.2~1.6 Fe(%): ≤2.0 Zr(%): 0.02~0.08 B(%): 0.003~0.010 | C(%): ≤0.06 Ti(%): ≤3.0 Co(%): ≤13.0 Al(%): ≤1.25 Fe(%): ≤2.0 | 
 
  
Waspaloy / UNS N07001 Mechanical Properties
Tensile strength, Rm/MPa: ≥ 1100
 Yield strength, Rp/MPa: ≥ 760
Elongation/%: ≥ 20
 Reduction of area, ψ/%: --
Impact, KV /J: --
 Hardness, HBW: --
 
 Applications
Waspaloy (UNS N07001) is commonly used for compressors and rotor discs, shafts, washers, seals, rings and casings, fasteners, and various other engine hardware, airframe components, and missile systems.
If you are interested in our products or have any questions, please contact our team of engineers at
 sales@ss-bars.com
  
 

  
  
 
|   | 
| NiCr20Co13Mo4Ti3Al W-Nr 2.4654 Superalloy Waspaloy UNS N07001 Steel Bar Images | 
 DIN X20Cr13 1.4021 Turbine Blade Steel DIN X20Cr13 Round Bar DIN 1.4021 Flat Bar
                                                                                    
                        
                        
                        
                                                            DIN X20Cr13 1.4021 Turbine Blade Steel DIN X20Cr13 Round Bar DIN 1.4021 Flat Bar
                                                    
                        
                     ASTM XM-25 AMS 5773 Turbine Blade Steel ASTM XM-25 Round Bar AMS 5773 Flat Bar
                                                                                    
                        
                        
                        
                                                            ASTM XM-25 AMS 5773 Turbine Blade Steel ASTM XM-25 Round Bar AMS 5773 Flat Bar
                                                    
                        
                     Custom 450 UNS S45000 Turbine Blade Steel Custom 450 Round Bar UNS S45000 Flat
                                                                                    
                        
                        
                        
                                                            Custom 450 UNS S45000 Turbine Blade Steel Custom 450 Round Bar UNS S45000 Flat
                                                    
                        
                     ASTM 420 UNS S42000 Turbine Blade Steel For Engineering
                                                                                    
                        
                        
                        
                                                            ASTM 420 UNS S42000 Turbine Blade Steel For Engineering
                                                    
                        
                     Cold Drawn DIN 1.4923 Steel Square Steel Bar Flat Cold Working
                                                                                    
                        
                        
                        
                                                            Cold Drawn DIN 1.4923 Steel Square Steel Bar Flat Cold Working
                                                    
                        
                     Custom 450 Turbine Blade Steel XM-25 Round Bar S45000 Flat Bar AMS 5773 GD450
                                                                                    
                        
                        
                        
                                                            Custom 450 Turbine Blade Steel XM-25 Round Bar S45000 Flat Bar AMS 5773 GD450
                                                    
                        
                     A286 Turbine Blade Steel AISI 660 1.4980 Round Bar X6NiCrTiMoVB25-15 Bar S66286
                                                                                    
                        
                        
                        
                                                            A286 Turbine Blade Steel AISI 660 1.4980 Round Bar X6NiCrTiMoVB25-15 Bar S66286
                                                    
                        
                     AM 355 Turbine Blade Steel UNS S35500 Flat Bar Alloy AM-355 Bar ASTM Type 634
                                                                                    
                        
                        
                        
                                                            AM 355 Turbine Blade Steel UNS S35500 Flat Bar Alloy AM-355 Bar ASTM Type 634
                                                    
                        
                     DIN X12CrS13 1.4005 Turbine Blade Steel DIN X12CrS13 Round Bar 1.4005 Flat Bar
                                                                                    
                        
                        
                        
                                                            DIN X12CrS13 1.4005 Turbine Blade Steel DIN X12CrS13 Round Bar 1.4005 Flat Bar
                                                    
                        
                     DIN X20CrMoW12-1 1.4935 Turbine Blade Steel X20CrMoW12-1 Round Bar 1.4935 Flat
                                                                                    
                        
                        
                        
                                                            DIN X20CrMoW12-1 1.4935 Turbine Blade Steel X20CrMoW12-1 Round Bar 1.4935 Flat